مواقع التدريسيينجامعة الكوفة
0Publications

About

*B.D.S. 1999 Al-Anbar University
*M.Sc. 2012 Baghdad University
*Diploma 2015 British Academy of implant& restorative Dentistry
*Diploma 1986 Dental technician

Publications

11
July-September 2019

Comparison of Shear Bond Strength of Translucent Zirconia Veneers Bond to Enamel among Different Light Intensity (An in Vitro Study)

AuthorsSattar Hmedat1, Zuha Ayad Jaber1, Salah Mahdi Ibrahim2
JournalIndian Journal of Forensic Medicine & Toxicology,
Abstract

Abstract Objectives: the cosmetic dentistry request to increase the duration of veneers and crowns to the tooth structure, which increase the cosmetic translucent zirconia duration. Aims: the research objective is to Contrast of shear bond strength of translucent zirconia veneers bond to the enamel among changed light intensity. Method: thirty upper-removed premolar was used. Thirty translucent zirconia discs were made according to manufacturing direction then randomly dived into two assemblies. Using bisco choice2 resin cement is light cured. The two assemblies dropped into I group and II group, Group I: low intensity light power has at 1000mW / cm² (10 Sec) used. Group II: high light intensity groups that is high intensity power at 1400 mW/cm² (4 Sec) used. Results: high significant difference (<0.001) Statistically among groups II and I in means for low intensity assemblies is 10.12 Mpa however the high light intensity assemblies mean 16.97 Mpa. Conclusions: Giving to this study the high intensity light more efficient bond force of translucent zirconia veneer to the enamel than low intensity light.

April 13, 2017; Acce

Comparison of Shear Bond Strength of Composite to Composite Bond in Increment Technique (An in vitro study)

AuthorsSattar J. Abdul-Zahra Al Hmedat* , Zuha Ayad Jaber
JournalJournal of Dental and Oral Health
Abstract

Abstract Objective: Bonding composite to composite restorations in increment technique. The objective of this in vitro study was to determine the best procedure and bond to inhancing the bond between two incremente composite, by measuring shear bond strength between two new incremente composites, surfaces were treated with a bonding agent (Bond Universal [3M ESPE]), mechanical retention by roughening surface with diamond bur and air isolation of cured composite. Methods: Four groups and each group composed of 20 composite blocks The block prepared at dimension: (3, 3, 2 mm) made from 3M ESPE Nano Hybrid Z 250XT. First group: Oxygen -polymerization inhibited specimens (20 block). Second group: Inhibition formed of Oxygen - polymerization inhibited specimens (20 block) by using celluloid strip. Third group: all in one adhesive system (one bottle\self etching 3M ESPE single bond universal adhesion material which contained silane) specimens (20 block) Four group: grinding specimens (20 block) of composite by diamond bur. Using The VALO Cordless curing light has multi-wavelength (395 - 480nm) Light Emitting Diode (LED). Results: Experimental shear bond strengths Direct group 32.14 ± 1.148 (Mpa), Bond group 30.75 ± 1.854 (Mpa), celluloid Strip group 13.73 ± 1.301 (Mpa) and Grinding group 19.67 ± 1.919 (Mpa). The higher shear bond strength in direct and bond groups and non significant with lowest mean result of strip and grinding groups. was used to analyze data. One way ANOVA (F-test) was used to detect the significant differences between groups. L.S.D was used to compare mean differences between each two groups (multiple comparison). P≤0. 01 was considered to be significant at 1%. Conclusions: Depending on the mechanical property being tested, group treatments with all in one adhesive system (one bottle\self etching 3M ESPE single bond universal adhesion material and direct group produced different results. produced more consistent results than grinding and celluloid groups.

2025

Comparison of the shear bond strength between composite resin and enamel among different bonding procedure’s applications

AuthorsSattar Jabbar Abdul-Zahraa Al-Hmedata, Wurood Hashim Majeed Al-Ameedeea |Zuha Ayad Jabera Salah M. Ibrahim
JournalJournal of Medicinal and Pharmaceutical Chemistry Research
Date2025-01-10
Abstract

In dentistry, establishing a permanent bond between resin and tooth structure is essential for successful tooth restoration. While various factors affect bond strength, adhesive application time is often overlooked. This study investigated how the adhesive application time affects the bond strength between micro-filled resin and enamel when using 3M One Bond Universal Adhesive. Forty premolars were randomly selected. They were divided into four groups (10 in each group). They underwent 5, 10, 15, and 20 seconds of adhesive application time followed by a curing process. Shear bond strength was evaluated using a testing machine. There was a significant positive correlation between the application time of the adhesion promoter and shear bond strength. The group with the longest bonding time (20 seconds) had the highest mean shear bond strength (X MPa). Adequate bonding time is essential for optimal bond strength between composite resin and enamel. To ensure the long-term success of composite restorations, dentists should follow the manufacturer's recommendations on the duration of bonding application.

2025

The Effect of Enamel Roughness with Different Burs Preparation on The Adhesion of Resin Composite by Eighth-Generation Bonding Agent

AuthorsSattar Jabbar Abdul-Zahra Al Hmedat
JournalFrontline Medical Sciences and Pharmaceutical Journal
Date2025-05-26
Abstract

OBJECTIVE The aim study to evaluates the effect of different diamond bur roughness on the shear bond strength of resin-based composite to the enamel superficial microroughness This may affect adhesion by modifying the substrates' characteristics when using an eighth-generation bonding agent adhesive. MATERIALS AND METHODS The 40 premolars were embedded in acrylic resin blocks, Samples were distributed 10 Samples into 4 groups according to burs: black, white, yellow burs, and polishing (control) prepared buccally with in the enamel flat surface, followed applied by eighth-generation bonding agent and A heavy-body silicone mold was used to form an accurate template for composite application, applied with composite resin restoration and polymerization. Shear bond strength (SBS) was tested using a Zwick Roell universal testing machine, and failure modes were analyzed. RESULTS showed white bur group exhibited the highest shear bond strength (SBS), with a mean value of 0.80 ± 0.118 MPa followed by yellow bur group 0.54 ± 0.119 MPa, followed by black bur group showed of 0.40 ± 0.071 MPa, followed by pumice polishing group had the lowest bond strength, at 0.34 ± 0.053 MPa, significant differences between the 4 uses groups (P value < 0.001). CONCLUSION. enamel surface roughness created by white diamond burs considerably influences the shear bond strength of resin bonded restorations

2025

An Evaluation of Bacterial Inhibition on E-max and Zirconia Disks after Different Surface Treatments: A Comparative In vitro Study

AuthorsZahraa Abdulaali Al-Ibraheemi, Zanbaq Azeez Hanoon1 , Amal Qasim Ahmed3 , Sattar Jabbar Abdul-Zahra Al-Hmedat Salah M. Ibrahim2, *and Abtesam Imhemed Aljdaimi4
JournalThe Open Microbiology Journal
Date2025-04-25
Abstract

Abstract: Background: Comprehending how bacteria adhere to different materials is essential for ensuring the long-term success of dental restorations. Various types of ceramic dental materials with distinct chemical and mechanical properties have been developed for this purpose. Therefore, this in vitro study aimed to investigate bacterial inhibition on E-max and zirconia disks after different surface treatments. Materials and Methods: Forty discs of zirconia and 40 discs of lithium disilicate-pressed E-max were prepared with standardized dimensions. Each main group was divided into two subgroups (20 for each). One subgroup was subjected to polishing and glazing, while the second one was not. After thermocycling, discs in each subgroup were placed on the bacteria culture plates containing either Streptococcus mutans (S. mutans) or Escherichia coli (E. coli). Results: The zirconia polishing group achieved the greatest bacterial inhibition, followed by the polished E-max group. The glazed zirconia and glazed E-max groups had lower values and highly significant differences were found. Conclusion: Bacteria were more inhibited in the polished groups than in the glazed groups of both zirconia and E- max.

2024

Histological Study to Evaluate the Effect of Local Application of Myrtus Communis Oil on Alveolar Bone Healing in Rats

AuthorsSalah M. Ibrahim1, Sattar Jabbar Abdul-Zahra Al-Hmedat2
JournalThe Open Dentistry Journal
Date2024-06-18
Abstract

Abstract: Background: Reproving dental defects is still a significant problem in dentistry. Bone is a highly vascularized tissue that is reliant on maintaining skeletal structure. The medicinal properties of healthy and preventative herbs were recognized by both the ancient and modern pharmacists and doctors in medicine. The effects of Myrtus communis oil (M) are employed as a healing agent for bone loss with anti-inflammatory and antioxidant properties. The advantage of Myrtus communis oil (M) is that it is a form of osteoconduction in the process of bone healing, decreases pain, and decreases the length of time needed for bone healing. Aim: to identify the effectiveness of Myrtus communis oil's local application in healing bone defects; the author performed a histological analysis. Materials and Methods: This study involved 12 albino male rats weighing (300-400) grams, aged (6-8) months. The animals were subject to a surgical operation on the alveolar bone. The group of animals was divided into two distinct categories based on the applicable materials. Control group: 6 rats; bone defect was only washed by normal saline, and bone defect was left to heal normally. Myrtus communis group: 6 rats; bone defect treated by local application of 1 μl of Myrtus communis oil (M). The rats were sacrificed 7 and 14 days after surgery (six rats for each period). All bone sections stained with hematoxylin and eosin underwent a light microscope histological inspection, which included counting the number of bone cells (osteoblasts, osteocytes, and osteoclasts) and evaluating the results of histomorphometric analysis. Results: Histological and histomorphometric findings of the present study show the acceleration of bone defect healing process in the Myrtus communis group as the increase in mean count difference measured of osteoblast, osteocyte, and osteoclast with statistically significant in 7 days duration. The result shows the positive expression of osteoblast, osteocyte, and osteoclast in all groups, with the highest statistical difference in osteocyte mean number in the Myrtus communis group. Conclusion: Myrtus communis oil (M) has the potential to promote and be an effective therapeutic for the bone injury healing process. Keywords: Myrtus communis oil, Hematoxylin and eosin stain, Histomorphometrical analysis, Osteocyte, Osteoblast, LSD test.

2020

Effect of autoclave sterilisation and heat activated sodium hypochlorite irrigation on the performance of nickel-titanium rotary files against cyclic fatigue

AuthorsZuha Ayad Jaber, Sattar Jabbar Abdul-Zahra Al-Hmedat , Sarmad Adel Hameed , Suhad Jabbar Hamed Al-Nasrawi , Abtesam Imhemed Aljdaimi & Julfikar Haider
JournalAdvances in Materials and Processing Technologies
Date2020-11-25
Abstract

ABSTRACTThe present study aims to assess the impact of heat- activated sodium hypochlorite (NaOCl) and/or autoclave sterilisation on the cyclic fatigue resistance (CFR) of heat-treated nickel- titanium rotary files used in root canal treatment. The CFR of One Curve (OC) files was evaluated under the following conditions: as received (Group 1; control), immersion in NaOCl at 23 ± 1ºC (Group 2), immersion in NaOCl at 60 ± 1ºC (Group 3), autoclave sterilisation at 135 1ºC (Group 4), combined treatment of autoclave sterilisation and immersion in NaOCl at 23 ± 1ºC (Group 5), and combined treatment of autoclave sterilisation and immersion in NaOCl at 60 ± 1ºC (Group 6). A simulated root canal in a zirconia block was utilised to test the performance of the files. All the types of treatments resulted in significant reductions in fracture resistance of the OC files. Immersion of the files in NaOCl at 23ºC revealed the smallest reduction, while combined treatment of autoclaving and immersion in NaOCl at 60ºC caused the greatest reduction. Autoclave sterilisation or exposure of OC files to 2.5% NaOCl adversely affect the cyclic fatigue life and increasing solution temperature or combined treatment caused additionally significant reduction in CFR

2019

COMPARISON OF CYCLIC FATIGUE AMONG PROTAPERGOLD, ONE CURVE, WAVE ONE® GOLD AND VDW BLUE FILES

AuthorsSattar J. Abdul-Zahra Al Hmedat* , Zuha Ayad Jaber and Suhad Jabbar Al-Nasrawi
JournalBiochem. Cell. Arch. Vol. 19, No. 1, pp. 1309-1312, 2019
Abstract

AbstractABSTRACT : The reciprocating file program was claimed the resistance be increased to fatigue in evaluation with the rotation file program.Newly 2 new kinds of NiTi files have been marketed one curve file and VDW blue. The purpose of this study was to comparison of cyclic fatigue resistance amongProTaper gold, one curve, WaveOne® Gold and VDW blue files. Cyclic fatigue testedfour files with the zirconia artificial canal curve 45 canal a simultaneouspecking motion hasobtain with (n = 6 each) instrument that (operataccording to recommended reciprocationmotion until the ProTaper gold, one curve, WaveOne® Gold and VDW blue filesfractured . ProTaper F2 and one curve were tested incontinuous rotation and WaveOne® Gold and VDW blue files tested in reciprocation movement. (NCF) represent number ofcycles to fracture which obtain by measuring the time spend to fracture. Using one-way statisticanalysis. The results revealed that VDW blue had higherNCF&then One-curve and then WaveOne gold and the ProTaper gold F2 had a lowest NCF. Reciprocating files VDW blue demonstratedsignificantly higher cyclic fatigue than others files (P <0.01). The 2 brands of NiTi file VDW blue and One-curve appear to have superior mechanical properties than WaveOne gold and ProTaper gold F2.

2017; 29(2):33-41)

A Comparison of Vertical Marginal Fit of different Brands of Translucent Zirconia Crown Restorations

AuthorsSattar J. Abdul-Zahra Al Hmedat, B.D.S., M.Sc. (1), لايوجد
JournalJ Bagh College Dentistry
Abstract

ABSTRACT Background: As the development of zirconia crown using CAD/CAM technology, the usage of full zirconia crown is gradually increased. The aim of this in-vitro study was to evaluate and contrast the vertical marginal fit of single allceramic translucent zirconia crowns constructed from different brands translucent zirconia blanks. Materials and Methods: An acrylic resin model of a left maxillary premolar was prepared all around the tooth with (1 mm) depth and 3D scanning to get fifteen STL files, then distributed into three groups (Imes-icor, Whitepeaks and Dental direct), 3D scanning and milling machine by Imes-icor CAD/CAM devise. Marginal gaps along vertical planes were measured at four indentations at the (mid mesial, mid distal, mid buccal, mid palatal) using a light microscope at a magnification of x100. One-way ANOVA, LSD tests were performed to determine the mean and standard deviation of the three blanks groups. Results: Statistically high significant difference (p < 0.00) was found between the groups. The marginal gap value of the groups varied Whitepeaks crowns was (105.42 ± 7) μm, which was significantly higher than the two overall mean marginal gap measured for the Imes-icor crowns (59.3 ± 4) μm and Dental direct crowns (54.5 ± 4.9) μm, the Dental direct which was lowers overall mean vertical gap measurement. Conclusions: The marginal gap values of Dental direct crowns is considerably lower than that of Whitepeaks crown, The marginal gap values of all the groups made of monolithic high translucent Y-TZP demonstrated acceptable marginal gaps values. Key words: Vertical marginal fit, crown, zirconia. . (J Bagh Coll Dentistry 2017; 29(2):33-41)

2016

A comparison of fracture strength among different brands of translucent zirconia crown restorations

AuthorsDr. Sattar J. Abdul-Zahra Al Hmedat* B.D.S, M.Sc. Department of conservative Dentistry, College of Dentistry, University of Kufa, Najaf, Iraq., Dr. Zuha Ayad Jaber B.D.S., M.Sc. Department of conservative Dentistry, College of Dentistry, University of Kufa, Najaf, Iraq. DR. Adel F. Ibraheem B.D.S, M.Sc. Department of Conservative Dentistry, College of Dentistry, University of Baghdad, Baghdad, Iraq.
JournalJournal of Biology, Agriculture and Healthcare
Abstract

Abstract: Objectives: As the development of translucent zirconia crown using CAD/CAM technology, the usage of full zirconia crown is gradually increased. The purpose of this study was to investigate the highest fracture strength of translucent zirconia full zirconia crowns among different brands of translucent zirconia. Methods: Maxillary 1stpremolar resin teeth were prepared the total circumferential axial reduction was about (1 mm), and axial taper of 6°. Three brands of translucent zirconia (Whitepeaks, Imes-icor and Dentaldirect) that was used in three groups, every group contain five full zirconia crowns using CAD/CAM system (CAD/CAM system 250i, Imesicor, Germany). The samples seated on the resin die using. All specimens were tested with a universal testing machine. Single load-to-fracture was applied on the lingual aspect of the facial cusp at a rate of 1mm/min. The specimens were thoroughly evaluated for bulk fracture with fractography. Results: Statistically high significant difference (p < 0.00) was found between the groups. The fracture strength of the groups varied Whitepeaks crowns was (2737.5 ± 106) N, which was significantly higher than the two overall mean fracture strength measured for the Imes-icor crowns (3620 ± 40) N and Dental direct crowns (3830 ± 130) N, the Dental direct highest fracture strength than other groups. Conclusions. The fracture strength of Dental direct crowns is considerably higher than that of Whitepeaks crown, The fracture strength of all the groups made of monolithic high translucent Y-TZP is exceeded human maximum bite force, sufficient for clinical use for the majority of patients.

2015,4

A comparison of vertical marginal fit of three different types of all ceramic crown restorations (An In vitro study)

AuthorsAdel F. Ibraheem, Sattar J.A. Hmedat
JournalJournal of Gene c and Environmental Resources Conserva on, 2015, 3(1):84-92.
Abstract

The objective of this in vitro study was to evaluate and compare the vertical marginal fit of crowns fabricated with three different techniques: ZrO2 CAD/CAM,ZO2; copy-milling machine and Lithium disilicate pressable ceramic, before and after porcelain firing cycles and after glaze cycles. An acrylic resin model of a left maxillary first molar was prepared and duplicated to have Nickel-Chromium master die. Thirty die stone dies were distributed randomly (10 dies for each group), group(I) system, copy milling (Amann Girrbach), group(II) heat pressable ceramic(Neytech system)and group(III) CAD/CAM (Amann Girrbach). Marginal gaps along vertical planes were measured at four indentations at the (mid mesial, mid distal, mid buccal, mid palatal) before (Time 0) and a er porcelain firing cycles(Time 1) and a er glaze cycles(Time 2) using a light microscope at a magnifica on of ×100. One way ANOVA LSD tests were performed to determine whether the mean and standard deviation of sub group Time 2 between the three systems. Results revealed that the mean values of the group(III) Time 0 were (6.77μm), Time 1(8.75μm) and Time 2(10.62 μm), group(I) Time 0 (151.95μm), Time 1(157.37μm) and Time 2(159.52 μm) , and group(II) Time 0 (55.35μm), Time 1(63.85μm) and Time 2(65.55 μm). One way ANOVA test revealed quantitative differences of the three groups. Comparing the mean values of marginal gap of the three tested groups at Time 2 revealed highly sta s cal significance(P<0.01).

View details